If a third party galvanizes
Recommended
Use ambient-temperature hydrochloric acid, and keep pickling under ten minutes.
Hold the zinc bath at a constant temperature.
Shot or sand blast any added steel (stringers, support angles, stiffeners) before galvanizing, and make sure it's de-scaled and rust free.
Space pieces apart on the rack so the pickling heat does not create hot spots.
Keep material inside and wrapped so surface rust cannot form.
Not recommended
Leaving material in acid pickling for more than ten minutes.
Using a heated sulfuric acid immersion for more than three minutes.
An inconsistent zinc bath temperature.
Supplying greasy, scaly or rusty material to the galvanizer.
Exposure to the elements before galvanizing.
Drilling or welding after galvanizing.
Disclaimer
If the SLIPNOT surface is galvanized incorrectly, the surface can be compromised. Traction Technologies Holdings, LLC is not liable for damage to the SLIPNOT surface by third parties, or for replacing or repairing material drilled or welded after galvanizing.
Pieces damaged in material handling must be repaired in the field. Surfaces that are not repaired and protected will fail prematurely.